High-carbon steels are susceptible to hydrogen induce cracking because they are with high content of ().
A. carbon
B. sulphur
C. chromium
D. nickel
E. 2-1-2
F. 期末
查看答案
After welding, QTLA steels can be tempered automatically because they possess () martensite transformation starting temperature and the cooling rate is ()
A. high/slow
B. high/rapid
C. low/slow
D. low/rapid
E. 2-2-1
F. 期末
Some types of QTLA steels are susceptible to liquation cracking because they contain a lot of ().
A. Ni
B. P
C
D. Cr
E. 2-2-2
F. 期末
To avoid hydrogen induced cracking, we have to limit the intrusion of () during welding.
A. H
B. C
C. S
D. P
E. 2-1-2 2-2-2 2-3-2
F. 期末
Comparing with QTLA steels, HTLA steels are with () hardness and () toughness.
A. higher/lower
B. higher/higher
C. lower/lower
D. lower/higher
E. 2-3-1
F. 期末