To avoid hydrogen induced cracking, we have to limit the intrusion of () during welding.
A. H
B. C
C. S
D. P
E. 2-1-2 2-2-2 2-3-2
F. 期末
查看答案
Comparing with QTLA steels, HTLA steels are with () hardness and () toughness.
A. higher/lower
B. higher/higher
C. lower/lower
D. lower/higher
E. 2-3-1
F. 期末
HTLA steels are susceptible to reheat cracking because they contain a lot of ()
A. carbides
B. H
C. S
D. P
E. 2-3-2
F. 期末
To avoid liquation cracking, during the welding of HTLA steels, we'd better to pay attention to the content ratio of () to ()
A. Ni/Mn
B. Ni/Si
C. Mn/Si
D. Si/C
E. 2-3-2
F. 期末
HTLA steels are ().
A. medium carbon
B. low carbon
C. high alloy
D. high carbon
E. 2-3-1
F. 期末